Influence of firing conditions and production methods on fracture strength of titanium-based metal ceramic crowns
Malmö University, Faculty of Odontology (OD).
Commercial Dental Laboratory, Malmö, Sweden.
Department of Chemistry and Chemical Engineering, Chalmers University of Technology, Gothenburg, Sweden.
Malmö University, Faculty of Odontology (OD).ORCID iD: 0000-0001-6593-0151
2018 (English)In: Journal of Adhesion Science and Technology, ISSN 0169-4243, E-ISSN 1568-5616, Vol. 32, no 3, p. 225-238Article in journal (Refereed) Published
Abstract [en]

Objectives: This study evaluated the effect of argon atmosphere compared with vacuum during porcelain firing on the fracture strength of crowns made of porcelain and electron beam melted (EBM) Ti-6Al-4 V, cast commercially pure titanium or milled commercially pure titanium. Methods: Sixty crown copings of c. p. titanium, Ti-6Al-4 V alloy and porcelain were fabricated using three production techniques. The copings were fired either under vacuum or in an argon gas atmosphere. Specimens were subdivided into groups of cast c. p. titanium, milled c. p. titanium and EBM Ti-6Al-4 V which were further subdivided according to firing modes employing either vacuum or argon gas. The 60 specimens were subjected to cyclic preloading and thermocycling, and were then individually loaded until interface fractured. Differences between the group mean values were calculated using the one-way ANOVA and Tukey's range test. Two fractured samples from each group were cut with a diamond blade and examined using SEM and EDS for visualization and chemical composition analysis of the fractured interface. Results: The highest mean fracture strength values, though not significant, were recorded for the groups fired in argon atmosphere, and the lowest mean fracture strength values were recorded for the groups fired in vacuum, with one exception. Comparing the two main groups of firing atmosphere, no significant difference could be documented. SEM and EDS analysis indicated clear differences in composition and structure between the groups included in the study. Conclusions: Firing in argon atmosphere does not significantly improve the fracture strength of porcelain bonded to titanium.

Place, publisher, year, edition, pages
Taylor & Francis, 2018. Vol. 32, no 3, p. 225-238
Keywords [en]
Titanium, dental ceramics, dental porcelain, bond strength, argon
National Category
Natural Sciences
Identifiers
URN: urn:nbn:se:mau:diva-5965DOI: 10.1080/01694243.2017.1352119ISI: 000428110700001Scopus ID: 2-s2.0-85025127936Local ID: 26630OAI: oai:DiVA.org:mau-5965DiVA, id: diva2:1402852
Available from: 2020-02-28 Created: 2020-02-28 Last updated: 2024-06-17Bibliographically approved

Open Access in DiVA

No full text in DiVA

Other links

Publisher's full textScopus

Authority records

Vult von Steyern, Per

Search in DiVA

By author/editor
Vult von Steyern, Per
By organisation
Faculty of Odontology (OD)
In the same journal
Journal of Adhesion Science and Technology
Natural Sciences

Search outside of DiVA

GoogleGoogle Scholar

doi
urn-nbn

Altmetric score

doi
urn-nbn
Total: 76 hits
CiteExportLink to record
Permanent link

Direct link
Cite
Citation style
  • apa
  • ieee
  • modern-language-association-8th-edition
  • vancouver
  • Other style
More styles
Language
  • de-DE
  • en-GB
  • en-US
  • fi-FI
  • nn-NO
  • nn-NB
  • sv-SE
  • Other locale
More languages
Output format
  • html
  • text
  • asciidoc
  • rtf